Close

Site Information

Material Specs

ADVANCED OZONE RESISTANCE tested to...

EPDM

   70 hour @ 500pphm 

SILICONE

   70 hour @ 500pphm 

HIGH TEMPERATURE RESISTANCE

Tested to                                  Intermittent

                                                 Continuous

 

+135°C (+275°F)

+100°C (+212°F)

 

+260°C (+500°F)

+225°C (+437°F)

LOW TEMPERATURE RESISTANCE tested to... -55°C      (-67°F) -74°C      (-101°F)
COMPRESSION SET minimum... 25% 50%